| Specification | C%: Mn%; 0.07∽0.25: 1,00 Max; Tempering Temperature (°C): Tensile Strength (MPa); Annealed *: 655; 204: 1600; 316: 1580; 427: 1620; 538: 1305; 593: 1035; 650: 895; Grade: Reasons for choosingHIGH CARBON 420 STAINLESS STEEL; 410: Only a lower NMened strength is needed. |
|---|